Hordhac

Iyadoo horumarinta warshadaha baabuurta, suuqa loogu talagalay alwaaxyada aluminium ee saameynta alwaaxyada ayaa sidoo kale si degdeg ah u koraya, inkastoo ay weli yar yihiin cabbirka guud. Marka loo eego saadaasha Isbahaysiga Hal-abuurka Tiknoolajiyada Fudud ee Fudud ee Suuqa Saamaynta aluminiumka aluminium ee Shiinaha, marka la gaaro 2025, baahida suuqa waxaa lagu qiyaasaa inay ku dhowdahay 140,000 tan, iyadoo cabbirka suuqa la filayo inuu gaaro 4.8 bilyan RMB. Marka la gaaro 2030, baahida suuqa ayaa la saadaalinayaa inay noqoto ku dhawaad ​​220,000 oo tan, iyadoo lagu qiyaasay cabbirka suuqa ee 7.7 bilyan RMB, iyo kororka kobaca sanadlaha ah ee ku saabsan 13%. Isbeddelka horumarinta miisaanka khafiifka ah iyo kobaca degdegga ah ee moodooyinka baabuurta ee dhexdhexaadka ah ilaa-dhamaadka sare ayaa ah arrimo muhiim ah oo wadista horumarinta alwaaxyada saameynta aluminium ee Shiinaha. Rajada suuqa ee santuuqyada shilalka baabuurka ee saamaynta baabuurta ayaa rajo leh.

Marka kharashku hoos u dhaco oo tignoolajiyadu kor u kacdo, alwaaxyada aluminiumka saamaynta hore ee saamaynta hore iyo sanduuqyada shilalka ayaa si tartiib tartiib ah u sii faafaya. Waqtigan xaadirka ah, waxaa loo isticmaalaa moodooyinka baabuurta dhex-ilaa-dhamaadka sare leh sida Audi A3, Audi A4L, BMW 3 series, BMW X1, Mercedes-Benz C260, Honda CR-V, Toyota RAV4, Buick Regal, iyo Buick LaCrosse.

Ilaysyada aluminium aluminiumka ah ee saamaynta ku leh waxay inta badan ka kooban yihiin biraha isdhaafka ah ee saamaynta leh, sanduuqyada shilalka, sariiraha korka, iyo gacan-jiidashada gacmaha, sida ku cad sawirka 1.

1694833057322

Jaantuska 1: Aluminium Alloy Impact Beam Assembly

Sanduuqa shilku waa sanduuq bir ah oo ku yaala inta u dhaxaysa laydhka saamaynta iyo labada laydh ee dheer ee gaadhiga, oo asal ahaan u adeegaya sidii weel tamar nuugaya. Tamartani waxa ay tilmaamaysaa xoogga saamaynta. Marka baabuurku uu la kulmo shil, laydhka saamayntu waxa uu leeyahay heer go'an oo ah awoodda nuugista tamarta. Si kastaba ha noqotee, haddii tamartu ka badato awoodda iftiinka saameynta, waxay tamarta u wareejin doontaa sanduuqa shilka. Sanduuqa shilku waxa uu nuugaa dhammaan xoogga saamaynta oo is beddela, isaga oo hubinaya in laydhyada dhaadheer ay yihiin kuwo aan waxyeello lahayn.

1 Shuruudaha Alaabta

1.1 Cabbiradu waa inay u hoggaansamaan shuruudaha dulqaadka sawirka, sida ku cad sawirka 2.

 

1694833194912
Jaantuska 2: Qaybta Shilalka
1.2 Xaaladda Qalabka: 6063-T6

1.3 Shuruudaha Waxqabadka Makaanikada:

Xoogga Jilitaanka: ≥215 MPa

Xoogga Wax-soo-saarka: ≥205 MPa

Kordhinta A50: ≥10%

1.4 Waxqabadka Sanduuqa Shilalka:

Iyada oo la adeegsanayo dhidibka X-baabuurka, iyada oo la adeegsanayo dusha isku dhaca oo ka weyn qaybta isku-tallaabta alaabta, ku rar xawli dhan 100 mm/daqiiqo ilaa la burburiyo, oo leh qadar cadaadis ah 70%. Dhererka hore ee profile waa 300 mm. Marka la eego isku xirka feeraha xoojinta iyo derbiga dibadda, dildilaaca waa in ka yar 15 mm si loo arko in la aqbali karo. Waa in la hubiyaa in dildilaaca la oggol yahay aanu wax u dhimayn awoodda tamarta nuugista ee profile, waana in aanay jirin dildilaacyo la taaban karo oo meelaha kale ka dib markii la burburiyo.

2 Habka Horumarinta

Si aad isku mar u buuxiso shuruudaha waxqabadka farsamada iyo burburinta waxqabadka, habka horumarinta waa sida soo socota:

Adeegso usha 6063B oo leh halabuurka daawaha aasaasiga ah ee Si 0.38-0.41% iyo Mg 0.53-0.60%.

Samee hawo deminta iyo gabowga macmalka ah si loo gaaro xaaladda T6.

Shaqaalaysii ceeryaamo + hawo deminta oo samee daawaynta gabowga si aad u gaadho xaalada T7.

3 Wax soo saar tijaabo ah

3.1 Shuruudaha ka saarista

Wax soo saarka waxaa lagu fuliyaa on 2000T saxafiyiinta extrusion ah oo leh saamiga extrusion of 36. Qalabka loo isticmaalo waa ul aluminium homogenized 6063B. Heerkulka kuleylka usha aluminiumku waa sida soo socota: Aagga IV 450-III aagga 470-II aagga 490-1 aagga 500. Cadaadiska ugu weyn ee dhululubada wuxuu ku dhow yahay 210 bar, oo leh wajiga extrusion xasilloon oo leh cadaadis extrusion ku dhow 180 bar. . Xawaaraha usheeda dhexe waa 2.5 mm/s, iyo xawaaraha extrusion profile waa 5.3 m/min. Heerkulka meesha laga saaro waa 500-540 ° C. Deminta waxaa lagu sameeyaa iyadoo la isticmaalayo qaboojin hawo leh awoodda taageeraha bidix oo ah 100%, awoodda taageeraha dhexe 100%, iyo awoodda taageeraha midig 50%. Celceliska heerka qaboojinta ee aagga deminta wuxuu gaaraa 300-350°C/daqiiqo, heerkulka ka dib marka uu ka baxo aagga deminta waa 60-180°C. Ceeryaanka + hawo deminta, celceliska heerka qaboojinta ee aagga kuleylku wuxuu gaaraa 430-480C/daqiiqo, heerkulka ka dib marka laga baxo aagga deminta waa 50-70 ° C. Muuqaalka muuqaalku ma muujinayo foorarsi muhiim ah.

3.2 Gabow

Iyadoo la raacayo habka gabowga ee T6 ee 185 ° C ilaa 6 saacadood, adkaanta walxaha iyo sifooyinka farsamada waa sida soo socota:

1694833768610

Marka loo eego habka gabowga ee T7 ee 210 ° C 6 saacadood iyo 8 saacadood, adkaanta walxaha iyo sifooyinka farsamada waa sida soo socota:

4

Iyada oo ku saleysan xogta tijaabada, ceeryaamo + habka daminta hawada, oo ay weheliso habka gabowga ee 210 ° C/6h, waxay buuxisaa shuruudaha waxqabadka farsamada iyo tijaabinta burburinta labadaba. Iyadoo la tixgalinayo wax ku oolnimada, ceeryaamo + habka daminta hawada iyo habka gabowga 210°C/6h ayaa loo xushay wax soo saarka si loo buuxiyo shuruudaha sheyga.

3.3 Tijaabada Burburinta

Ulaha labaad iyo saddexaad, cidhifka madaxa ayaa la gooyaa 1.5m, dabada dabada waxaa la gooyaa 1.2m. Laba shaybaar midkiiba waxaa laga soo qaadayaa madaxa, dhexe iyo qaybaha dabada, dhererkooduna yahay 300mm. Tijaabooyinka burburinta waxaa la sameeyaa ka dib da'da 185 ° C / 6h iyo 210 ° C / 6h iyo 8h (xogta farsamada farsamada sida kor ku xusan) ee mashiinka baaritaanka walxaha caalamiga ah. Tijaabooyinku waxa lagu qaadaa xawaare dhan 100 mm/daqiiqo oo ay ku jirto qadar cadaadis ah 70%. Natiijooyinku waa sida soo socota: ceeryaamo + hawo deminta habsocodka gabowga ee 210 ° C / 6h iyo 8h, tijaabooyinka burburinta waxay buuxiyaan shuruudaha, sida ku cad Jaantuska 3-2, halka shaybaarada hawada-demiyay ay muujinayaan dildilaaca dhammaan hababka gabowga. .

Iyada oo ku saleysan natiijooyinka tijaabada burburinta, ceeryaamo + hawo deminta 210°C/6h iyo 8h hababka gabowga ayaa la kulma shuruudaha macmiilka.

1694834109832

Jaantuska 3-1: Dilaaca daran ee Hawada Demisay, Aan U Hogaansanayn Jaantuska 3-2: Wax Dilaac ah oo Ceeryaamo ah + Hawo Demisay, Waafaqsan

4 Gabagabo

Hagaajinta geeddi-socodka deminta iyo gabowga ayaa muhiim u ah horumarka guusha leh ee badeecada waxayna siisaa hab-socodka ugu habboon ee badeecada sanduuqa shilka.

Tijaabo ballaaran, waxaa la go'aamiyay in xaaladda walxaha alaabta sanduuqa shilka ay tahay 6063-T7, habka deminta waa ceeryaamo + qaboojinta hawada, iyo geeddi-socodka gabowga ee 210 ° C / 6h waa doorashada ugu fiican ee soo saarista ulaha aluminium Heerkulka u dhexeeya 480-500C, Xawaaraha usheeda dhexe ee 2.5 mm/s, extrusion heerkulka dhimanaya 480C, iyo heerkulka extrusion outt 500-540C.

Waxaa tafatiray May Jiang oo ka socota MAT Aluminum